Mechanical Properties Metric English Comments
Tensile Modulus 14.2 GPa

@Temperature 23.0 °C
2060 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)
Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 14.2 GPa

@Temperature 120 °C
2060 ksi

@Temperature 248 °F
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 14.2 GPa

@Temperature 23.0 °C
2060 ksi

@Temperature 73.4 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 14.2 GPa

@Temperature 25.0 °C
2060 ksi

@Temperature 77.0 °F
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization
Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive ..