Mechanical Properties Metric English Comments
Tensile Modulus 126.2 GPa

@Temperature 24.0 °C
18300 ksi

@Temperature 75.2 °F
Hexcel® HexPly® F155 Epoxy Resin, T2C145 Carbon Tape
Hexcel designation: TXX145-12"-F155; Various fibersInformation provided by HexCel
Tensile Modulus 126.2 GPa

@Temperature 93.0 °C
18300 ksi

@Temperature 199 °F
Dry
Hexcel® HexPly® F593 Epoxy Resin, T2G190 Carbon Tape
Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel
Tensile Modulus 126.2 GPa

@Temperature -54.0 °C
18300 ksi

@Temperature -65.2 °F
Dry
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape
Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel