Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1.00 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.00 GPa

@Temperature 90.0 °C
145 ksi

@Temperature 194 °F
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Tensile Modulus 1.00 GPa

@Temperature 90.0 °C
145 ksi

@Temperature 194 °F
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle..
Tensile Modulus 1.00 GPa

@Temperature 90.0 °C
145 ksi

@Temperature 194 °F
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Modulus 1.00 GPa

@Temperature 90.0 °C
145 ksi

@Temperature 194 °F
LATI Latan 2 POM
Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Tensile Modulus 1.00 GPa

@Temperature 60.0 °C
145 ksi

@Temperature 140 °F
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;..
Tensile Modulus 1.00 GPa

@Temperature 70.0 °C
145 ksi

@Temperature 158 °F
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Tensile Modulus 1.00 GPa

@Temperature 260 °C
145 ksi

@Temperature 500 °F
ASTM D 638
Saint-Gobain Meldin® 2021 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Tensile Modulus 1.00 GPa

@Temperature 90.0 °C
145 ksi

@Temperature 194 °F
LATI Later 4-V0 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L..
Tensile Modulus 1.00 GPa

@Temperature 120 °C
145 ksi

@Temperature 248 °F
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant
Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re..
Copyright © lookpolymers.com All Rights Reserved