Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.500 - 0.600 GPa @Temperature 23.0 °C |
72.5 - 87.0 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |