Polymer Property : Tensile Modulus = 0.500 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.500 GPa

@Temperature 150 °C
72.5 ksi

@Temperature 302 °F
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Modulus 0.500 GPa

@Temperature 150 °C
72.5 ksi

@Temperature 302 °F
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi..
Tensile Modulus 0.500 GPa

@Temperature 60.0 °C
72.5 ksi

@Temperature 140 °F
LATI Latamid 66 E21 PA 66, Impact Modified
Polyamide 66 (PA66). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
Tensile Modulus 0.500 GPa

@Temperature 120 °C
72.5 ksi

@Temperature 248 °F
LATI Latamid 66 PA 66
Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 0.500 GPa

@Temperature 90.0 °C
72.5 ksi

@Temperature 194 °F
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i..
Tensile Modulus 0.500 GPa

@Temperature 120 °C
72.5 ksi

@Temperature 248 °F
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 0.500 GPa

@Temperature 90.0 °C
72.5 ksi

@Temperature 194 °F
LATI Latan 13E71 POM
Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided ..
Tensile Modulus 0.500 GPa

@Temperature 90.0 °C
72.5 ksi

@Temperature 194 °F
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;..
Tensile Modulus 0.500 GPa

@Temperature 90.0 °C
72.5 ksi

@Temperature 194 °F
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled
Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Tensile Modulus 0.500 - 0.600 GPa

@Temperature 23.0 °C
72.5 - 87.0 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D1708
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)  (discontinued **)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis..
Tensile Modulus 0.500 GPa

@Temperature 70.0 °C
72.5 ksi

@Temperature 158 °F
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..