Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 862 MPa @Thickness 127 - 152 mm |
125000 psi @Thickness 5.00 - 6.00 in |
Aquamet 22 HS |
Crucible Steel Aquamet® 22 Stainless Steel AQUAMET 22 is a high-alloy stainless steel with superior corrosion resistance along with excellent toughness and high strength. It has higher strength than AQUAMET 17 in 3/4" to 1-1/4" dia., and it .. |