Polymer Property : Tensile Strength, Ultimate = 19100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 132 MPa

@Temperature 870 °C
19100 psi

@Temperature 1600 °F
Hot-Rolled Plate, Solution-Annealed
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy
INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex..
Tensile Strength, Ultimate 132 MPa

@Temperature 23.0 °C
19100 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Tensile Strength, Ultimate 132 MPa

@Temperature 80.0 °C
19100 psi

@Temperature 176 °F
Absolute Drying; ASTM-D638
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..