Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 132 MPa @Temperature 870 °C |
19100 psi @Temperature 1600 °F |
Hot-Rolled Plate, Solution-Annealed |
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |
|||
Tensile Strength, Ultimate | 132 MPa @Temperature 23.0 °C |
19100 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 132 MPa @Temperature 80.0 °C |
19100 psi @Temperature 176 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |