Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 115 MPa @Temperature 980 °C |
16700 psi @Temperature 1800 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature 1000 °C |
16700 psi @Temperature 1830 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature -40.0 °C |
16700 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.3%); ASTM-D638 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature 23.0 °C |
16700 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.7%); ASTM-D638 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature 80.0 °C |
16700 psi @Temperature 176 °F |
Practical Use (Water Absorption 1.25%); ASTM-D638 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature -40.0 °C |
16700 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D638 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature 23.0 °C |
16700 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.6%); ASTM-D638 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Tensile Strength, Ultimate | 115 MPa @Temperature 1000 °C |
16700 psi @Temperature 1830 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |