Polymer Property : Peel Strength = 8.00 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 8.00 - 12.0 kN/m
45.6 - 68.5 pli
ISO 4578
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Peel Strength 8.00 kN/m
45.6 pli
Impact Peel
Dow BETAMATE™ XW 1044-3 Epoxy
BETAMATE™ XW 1044-3 is a one component, epoxy based adhesive especially developed for the body shop. The adhesive can be applied by robot systems and it shows high adhesion to metal and non-metal ..
Peel Strength 8.00 kN/m
45.6 pli
Impact Peel
Dow BETAMATE™ XW 1185 Epoxy
BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi..