Polymer Property : Peel Strength = 6.40 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 5.60 - 6.40 kN/m
32.0 - 36.5 pli
Cured for 1 hr at 80°C
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..