Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 5.60 - 6.40 kN/m | 32.0 - 36.5 pli | Cured for 1 hr at 80°C |
Permabond ET5401 Epoxy Resin PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo.. |
|||
Peel Strength | 5.61 kN/m | 32.0 pli | Bell Peel Adhesion, Aluminum Etched, Cohesive Failure; ASTM D3167 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Peel Strength | 5.61 kN/m @Temperature 23.0 °C |
32.0 pli @Temperature 73.4 °F |
Bell Pell Adhesion, Aluminum Etched, Cohesive Failure; ASTM D3167 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |