Dow Corning 737 NEUTRAL CURE SEALANT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 737 NEUTRAL CURE SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RTV adhesive/sealant with primerless adhesion to most materialsInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 33
33
Tensile Strength, Ultimate 1.21 MPa
175 psi
Elongation at Break 300 %
300 %
Peel Strength 3.51 kN/m
20.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 22.0 °C
24.0 hour

@Temperature 71.6 °F
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance translucent
Color Black
White