Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.3836 kN/m | 2.188 pli | Adhesion |
Dielectric Polymers NT-580 Plating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Transparent adhesive allows easy precision alignmentFine line definitionClean tape removalGood conformabilityChemical resistantApp.. |
|||
Peel Strength | 0.3836 kN/m | 2.188 pli | Adhesion |
Dielectric Polymers NT-8512-2 Powder Coating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista.. |
|||
Peel Strength | 0.3836 kN/m | 2.188 pli | Adhesion |
Dielectric Polymers NT-9512 Powder Coating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista.. |
|||
Peel Strength | 0.3836 kN/m | 2.188 pli | Adhesion |
Dielectric Polymers NT-9512-2DL Selective Masking Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: High temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications: For selective masking appli.. |