Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 0.3836 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.3836 kN/m
2.188 pli
Adhesion
Dielectric Polymers NT-580 Plating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Transparent adhesive allows easy precision alignmentFine line definitionClean tape removalGood conformabilityChemical resistantApp..
Peel Strength 0.3836 kN/m
2.188 pli
Adhesion
Dielectric Polymers NT-8512-2 Powder Coating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista..
Peel Strength 0.3836 kN/m
2.188 pli
Adhesion
Dielectric Polymers NT-9512 Powder Coating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista..
Peel Strength 0.3836 kN/m
2.188 pli
Adhesion
Dielectric Polymers NT-9512-2DL Selective Masking Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: High temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications: For selective masking appli..
Copyright © lookpolymers.com All Rights Reserved