Material Notes:
Crosslinked silicone adhesive with polyester film backing.Features: High temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications: For selective masking applications where temperature resistance is critical.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Adhesive
50.8 microns
2.00 mil
Backing
50.8 microns
2.00 mil
PET film liner
Mechanical Properties Metric English Comments
Elongation at Break 90 %
90 %
Peel Strength 0.3836 kN/m
2.188 pli
Adhesion
8.77 kN/m
50.0 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
>= 260 °C
>= 500 °F
Shear Adhesive Failure (polyester failure)
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Breakdown 6500 V
6500 V
Dielectric Strength
Descriptive Properties Value Comments