Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated with oil typically used with machine parts.Information provided by 3M
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Carrier
68.6 microns
2.70 mil
Faceside Adhesive
68.6 microns
2.70 mil
Backside Adhesive
107 microns
4.20 mil
Caliper
150 microns
5.90 mil
Total Thickness
Mechanical Properties Metric English Comments
Peel Strength 0.93128 kN/m
5.3125 pli
ABS, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
1.10 kN/m
6.25 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
1.1504 kN/m
6.5625 pli
PP, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
1.3695 kN/m
7.8125 pli
ABS, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
1.380 kN/m
7.875 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
1.424 kN/m
8.125 pli
PC, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330
1.4791 kN/m
8.4375 pli
PP, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
1.808 kN/m
10.31 pli
PC, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Long term
149 °C
300 °F
Short term
Electrical Properties Metric English Comments
Dielectric Strength 47.2 kV/mm
1200 kV/in
Dielectric Breakdown 6900 V
6900 V
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 300LSE
Users viewing this material also viewed the following: