Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 10.6 - 10.6 g/25 mm @Temperature 66.0 - 66.0 °C |
10.6 - 10.6 g/in @Temperature 151 - 151 °F |
Average value: 10.6 g/25 mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |
|||
Seal Strength | 10.6 - 10.6 g/25 mm @Time 346000 - 346000 sec |
10.6 - 10.6 g/in @Time 96.0 - 96.0 hour |
Average value: 10.6 g/25 mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |