Seal Strength 10.6 - 10.6 g/25 mm

@Temperature 66.0 - 66.0 °C
10.6 - 10.6 g/in

@Temperature 151 - 151 °F
Average value: 10.6 g/25 mm Grade Count:6
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Seal Strength 10.6 - 10.6 g/25 mm

@Time 346000 - 346000 sec
10.6 - 10.6 g/in

@Time 96.0 - 96.0 hour
Average value: 10.6 g/25 mm Grade Count:6
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..