Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 10.6 g/25 mm @Temperature 66.0 °C, Time 346000 sec |
10.6 g/in @Temperature 151 °F, Time 96.0 hour |
Release Adhesion, 180° Peel, 80% RH; ASTM D1000 |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Seal Strength | 10.6 g/25 mm @Temperature 66.0 °C, Time 346000 sec |
10.6 g/in @Temperature 151 °F, Time 96.0 hour |
Release Adhesion, 180° Peel, 80% RH; ASTM D1000 |
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 10.6 g/25 mm @Temperature 66.0 °C, Time 346000 sec |
10.6 g/in @Temperature 151 °F, Time 96.0 hour |
Release Adhesion, 180° Peel, 80% RH; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 10.6 g/25 mm @Temperature 66.0 °C, Time 346000 sec |
10.6 g/in @Temperature 151 °F, Time 96.0 hour |
Release Adhesion, 180° Peel, 80% RH; ASTM D1000 |
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 10.6 g/25 mm @Temperature 66.0 °C, Time 346000 sec |
10.6 g/in @Temperature 151 °F, Time 96.0 hour |
Release Adhesion, 180° Peel, 80% RH; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 10.6 g/25 mm @Temperature 66.0 °C, Time 346000 sec |
10.6 g/in @Temperature 151 °F, Time 96.0 hour |
Release Adhesion, 180° Peel, 80% RH; ASTM D1000 |
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits.. |
|||
Seal Strength | 10.6 - 10.6 g/25 mm @Temperature 66.0 - 66.0 °C |
10.6 - 10.6 g/in @Temperature 151 - 151 °F |
Average value: 10.6 g/25 mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |
|||
Seal Strength | 10.6 - 10.6 g/25 mm @Time 346000 - 346000 sec |
10.6 - 10.6 g/in @Time 96.0 - 96.0 hour |
Average value: 10.6 g/25 mm Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |