Mechanical Properties Metric English Comments
1% Secant Modulus, TD 310 MPa
45000 psi
ISO 527-3
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50..
1% Secant Modulus, TD 310 MPa
45000 psi
ISO 527-3
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM-D882
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional ..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM-D882
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve..
1% Secant Modulus, TD 310 MPa
45000 psi
ASTM D882
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..