Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 310 MPa | 45000 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM-D882 |
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional .. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM-D882 |
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve.. |
|||
1% Secant Modulus, TD | 310 MPa | 45000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |