Mechanical Properties Metric English Comments
1% Secant Modulus, TD 182 MPa
26400 psi
ASTM D882
ExxonMobil LD 102.74 Thin Gauged Film Resin  (discontinued **)
LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical