Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 182 MPa | 26400 psi | ASTM D882 |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |