Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
LyondellBasell Petrothene® NA362176 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
LyondellBasell Petrothene® NA362005 Low Density Polyethylene ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
Westlake Mxsten CV77512 Polyethylene Plastomer Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM-D822 |
Westlake Mxsten CV77519 Polyethylene Plastomer Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin .. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
Westlake Mxsten CV77523 Polyethylene Plastomer Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this .. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 306.57 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 306.75 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LL 3001.32 Cast Film Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |