Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 96.5 MPa | 14000 psi | ASTM D882 |
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo.. |
|||
1% Secant Modulus, MD | 96.5 MPa | 14000 psi | D 882 |
Westlake EB591 9.0% Ethylene Vinyl Acetate Copolymer Westlake EB591 resin is a 9.0% EVA copolymer designed for ice bags, frozen food bags and other films that require excellent toughness and good heat sealing characteristics. This kosher compliant re.. |
|||
1% Secant Modulus, MD | 96.5 MPa | 14000 psi | ASTM-D882 |
Westlake Elevate™ EB591 9% EVA Copolymer Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl.. |
|||
1% Secant Modulus, MD | 96.5 MPa | 14000 psi | ASTM D882 |
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U.. |