Westlake EB591 9.0% Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Westlake Chemical Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EB591 9.0% Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake EB591 resin is a 9.0% EVA copolymer designed for ice bags, frozen food bags and other films that require excellent toughness and good heat sealing characteristics. This kosher compliant resin has excellent low temperature brittleness properties.Application/UsesFrozen packaging
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
D 1505
Melt Flow 2.0 g/10 min
2.0 g/10 min
D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 32.4 MPa
4700 psi
D 882
Film Elongation at Break, MD 300 %
300 %
D 1238
Film Elongation at Break, TD 950 %
950 %
D 882
Dart Drop 175 g/micron
4450 g/mil
D 1709
1% Secant Modulus, MD 96.5 MPa
14000 psi
D 882
1% Secant Modulus, TD 124 MPa
18000 psi
D 882
Optical Properties Metric English Comments
Haze 4.8 %
4.8 %
D1003
Gloss 60 %
60 %
At 45°; D 2457
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution