Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 78.6 MPa | 11400 psi | |
Abatron AboCast 8-18/Abocure 8-18 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Flexural Yield Strength | 78.6 MPa | 11400 psi | ASTM D790 |
Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Flexural Yield Strength | 78.6 MPa | 11400 psi | ASTM D790 |
PlastxWorld CEVIAN® S3500 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 78.6 MPa | 11400 psi | ASTM D790 |
PlastxWorld CEVIAN®-V 510 ABS High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |