Material Notes:
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.19 %
0.19 %
in 24 hours.
Viscosity Measurement 700
700
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Tensile Strength, Ultimate 42.75 MPa
6200 psi
Elongation at Break 2.4 %
2.4 %
Modulus of Elasticity 3.172 GPa
460.1 ksi
Flexural Yield Strength 78.6 MPa
11400 psi
Compressive Yield Strength 73.08 MPa
10600 psi
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 2.30e+9 ohm-cm

@Temperature 93.3 °C
2.30e+9 ohm-cm

@Temperature 200 °F
1.40e+11 ohm-cm

@Temperature 65.6 °C
1.40e+11 ohm-cm

@Temperature 150 °F
1.30e+15 ohm-cm

@Temperature 25.0 °C
1.30e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.81

@Frequency 1e+6 Hz
3.81

@Frequency 1e+6 Hz
Dissipation Factor 0.010

@Frequency 1e+6 Hz
0.010

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 2 weeks