PlastxWorld CEVIAN® S3500 PC/ABS alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® S3500 PC/ABS alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM 638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Yield Strength 78.6 MPa
11400 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
0.25 inch; ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in