Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical LG709W ABS, Low Gloss, Heat Resistance Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG.. |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Flexural Yield Strength | 70.6 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene GA850 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 70.6 MPa | 10200 psi | ASTM D790 |
Cheng Yu Plastic 3276 TPE Rubber |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM21M ABS Injection Molding Grade Medium Flow, Medium Impact, Medium RigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Flexural Yield Strength | 70.6 MPa @Thickness 6.40 mm |
10200 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Flexural Yield Strength | 70.6 MPa | 10200 psi | ASTM D790 |
RedEye On Demand Clear PolyJet™ FC720 for Rapid Prototyping Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offer.. |