Material Notes:
Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offers the best surface finish. These parts are built at a layer thickness of 16 microns (0.0006 inch or 0.01524mm) and can produce parts with fine feature detail.ApplicationsClear PolyJet Resin (FC720) works well for prototypes that require smooth surface finish and high feature detail. Parts from this material can absorb paint or dye, be chrome plated, used as a master for silicone molds and have been used in investment casting. Clear PolyJet parts will have a semi-translucent appearance, which can be enhanced with sanding and buffing. Typical industries included toys, foot wear, architecture and any industry where feature detail and surface finish our required.
Physical Properties Metric English Comments
Base Resin Density 1.092 g/cc
0.03945 lb/in³
Ash <= 0.010 %
<= 0.010 %
at 1000°C
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
Tensile Strength, Yield 42.3 MPa
6140 psi
ASTM D638
Elongation at Break 15 - 25 %
15 - 25 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Yield Strength 70.6 MPa
10200 psi
ASTM D790
Flexural Modulus 1.978 GPa
286.9 ksi
ASTM D790
Compressive Strength 69.4 MPa
10100 psi
ASTM D695
Izod Impact, Notched 0.250 - 0.380 J/cm
0.468 - 0.712 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 29.9 - 39.3 µm/m-°C

@Temperature 30.0 - 35.0 °C
16.6 - 21.8 µin/in-°F

@Temperature 86.0 - 95.0 °F
51.3 - 70.3 µm/m-°C

@Temperature 40.0 - 70.0 °C
28.5 - 39.1 µin/in-°F

@Temperature 104 - 158 °F
95.9 - 112.9 µm/m-°C

@Temperature 75.0 - 90.0 °C
53.3 - 62.72 µin/in-°F

@Temperature 167 - 194 °F
118.2 - 126.2 µm/m-°C

@Temperature 95.0 - 110 °C
65.67 - 70.11 µin/in-°F

@Temperature 203 - 230 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified