Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 66.9 - 141 MPa @Temperature 100 - 100 °C |
9700 - 20500 psi @Temperature 212 - 212 °F |
Average value: 104 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Flexural Yield Strength | 66.9 MPa | 9700 psi | ASTM D790 |
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |