Mechanical Properties Metric English Comments
Flexural Yield Strength 66.9 - 141 MPa

@Temperature 100 - 100 °C
9700 - 20500 psi

@Temperature 212 - 212 °F
Average value: 104 MPa Grade Count:2
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Flexural Yield Strength 82.0 - 141 MPa
11900 - 20500 psi
Average value: 120 MPa Grade Count:9
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..