Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 66.9 - 141 MPa @Temperature 100 - 100 °C |
9700 - 20500 psi @Temperature 212 - 212 °F |
Average value: 104 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Flexural Yield Strength | 82.0 - 141 MPa | 11900 - 20500 psi | Average value: 120 MPa Grade Count:9 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |