Mechanical Properties Metric English Comments
Flexural Yield Strength 45.0 - 52.0 MPa
6530 - 7540 psi
ASTM D790
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Flexural Yield Strength 23.0 - 52.0 MPa
3340 - 7540 psi
Average value: 33.7 MPa Grade Count:3
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..