Polymer Property : Flexural Yield Strength = 48900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 140 - 337 MPa

@Temperature -40.0 - 80.0 °C
20300 - 48900 psi

@Temperature -40.0 - 176 °F
Average value: 252 MPa Grade Count:1
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..