Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 20.7 - 48.0 MPa
3000 - 6960 psi
Average value: 30.0 MPa Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Flexural Yield Strength 21.0 - 48.0 MPa
3050 - 6960 psi
Average value: 36.6 MPa Grade Count:10
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..