Polymer Property : Flexural Yield Strength = 20.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 20.7 MPa
3000 psi
ASTM D790
Techmer ES Statiblend® PP CO 99054
Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.
Flexural Yield Strength 20.7 - 48.0 MPa
3000 - 6960 psi
Average value: 30.0 MPa Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..