Flexural Yield Strength 55.0 - 163 MPa
7980 - 23600 psi
Average value: 76.3 MPa Grade Count:8
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim..
Flexural Yield Strength 15.0 - 163 MPa

@Temperature 100 - 175 °C
2180 - 23600 psi

@Temperature 212 - 347 °F
Average value: 68.8 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..