Polymer Property : Flexural Yield Strength = 19500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 134 MPa
19500 psi
ASTM D790
NYCOA 2037 15% Glass Filled Nylon 6
15% glass filled very high viscosity nylon 6Information provided by NYCOA, Inc.
Flexural Yield Strength 134 - 185 MPa
19500 - 26800 psi
Average value: 156 MPa Grade Count:15
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Flexural Yield Strength 134 MPa
19500 psi
ASTM D790
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr..
Flexural Yield Strength 134 MPa
19500 psi
ASTM D790
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc.
Flexural Yield Strength 134 MPa
19500 psi
ASTM D790
PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld ..