Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 97.9 MPa
14200 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 134 MPa
19500 psi
ASTM D790
Flexural Modulus 5.98 GPa
867 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 6.35 mm
1.10 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 41.4 µm/m-°C

@Temperature 20.0 °C
23.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
Deflection Temperature at 1.8 MPa (264 psi) 134 °C
273 °F
0.25 inch; ASTM D648
Flammability, UL94 V-0

@Thickness 1.65 mm
V-0

@Thickness 0.0650 in
Copyright © lookpolymers.com All Rights Reserved