Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 47.6 - 117 MPa | 6900 - 17000 psi | Average value: 76.5 MPa Grade Count:43 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 18.6 - 117 MPa | 2700 - 17000 psi | Average value: 70.4 MPa Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 96.5 - 117 MPa | 14000 - 17000 psi | Average value: 107 MPa Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Flexural Yield Strength | 55.2 - 117 MPa | 8000 - 17000 psi | Average value: 90.3 MPa Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 57.0 - 117 MPa | 8270 - 17000 psi | Average value: 97.6 MPa Grade Count:13 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |