Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 47.6 - 117 MPa | 6900 - 17000 psi | Average value: 76.5 MPa Grade Count:43 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 47.6 MPa | 6900 psi | ASTM D790 |
Ineos ABS Lustran® 356 Extrusion, Low-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |