Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 75.8 - 82.7 MPa | 11000 - 12000 psi | ASTM D790 |
Novatec Novacycle® 501 PVC Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe.. |
|||
Flexural Yield Strength | 62.1 - 82.7 MPa | 9000 - 12000 psi | ASTM D790 |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Flexural Yield Strength | 79.0 - 83.0 MPa | 11500 - 12000 psi | Average value: 80.5 MPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 26.0 - 82.7 MPa | 3770 - 12000 psi | Average value: 40.2 MPa Grade Count:58 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |