Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Film Tensile Strength at Break, TD 53.1 MPa
7700 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..