Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 38.6 MPa | 5600 psi | ASTM D882 |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Film Tensile Strength at Break, TD | 38.6 MPa | 5600 psi | ASTM D882 |
ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A.. |
|||
Film Tensile Strength at Break, TD | 38.61 MPa | 5600 psi | ASTM D882 |
ExxonMobil HD 7925.30 Barrier Film Resin Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A.. |