ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications: Barrier Food PackagingBlown FilmFood packagingHeavy Duty BagsOriented Film ProductsSkin Layer for OPPStand Up PouchesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.965 g/cc
0.0349 lb/in³
ExxonMobil method
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 31.7 MPa
4600 psi
ASTM D882
Film Tensile Strength at Yield, TD 27.6 MPa
4000 psi
ASTM D882
Film Elongation at Break, MD 790 %
790 %
ASTM D882
Elmendorf Tear Strength MD 9.0 g
9.0 g
ASTM D1922
Elmendorf Tear Strength TD 200 g
200 g
ASTM D1922
Dart Drop Test <= 50.0 g
<= 0.110 lb
ASTM D1709A
Film Tensile Strength at Break, MD 24.8 MPa
3600 psi
ASTM D882
Film Tensile Strength at Break, TD 38.6 MPa
5600 psi
ASTM D882
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
1% Secant Modulus, TD 1520 MPa
220000 psi
ASTM D882