Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HD 7925.30 Barrier Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HD 7925.30 Barrier Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications: Barrier Food PackagingBlown FilmFood packagingHeavy Duty BagsOriented Film ProductsSkin Layer for OPPStand Up PouchesInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
ExxonMobil Method
Thickness 25.4 microns
1.00 mil
Melt Flow 2.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 31.72 MPa
4600 psi
ASTM D882
Film Tensile Strength at Yield, TD 27.58 MPa
4000 psi
ASTM D882
Film Elongation at Break, MD 790 %
790 %
ASTM D882
Film Elongation at Break, TD 6.0 %
6.0 %
ASTM D882
Elmendorf Tear Strength MD 9.0 g
9.0 g
ASTM D1922
Elmendorf Tear Strength TD 200 g
200 g
ASTM D1922
Dart Drop Test 50.0 g
0.110 lb
ASTM D1790
Film Tensile Strength at Break, MD 43.44 MPa
6300 psi
ASTM D882
Film Tensile Strength at Break, TD 38.61 MPa
5600 psi
ASTM D882
1% Secant Modulus, MD 1030 MPa
150000 psi
ASTM D882
1% Secant Modulus, TD 1520 MPa
220000 psi
ASTM D882
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved