Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 37.9 - 48.3 MPa
5500 - 7000 psi
ASTM D882
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film
Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
ASTM D882
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene
WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
ASTM D882
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
ASTM D882
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin
Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
ASTM D882
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
ASTM D882
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp..
Film Tensile Strength at Break, TD 37.9 MPa
5500 psi
ASTM D882
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film
Rogers 3001 bonding film is a thermoplastic chloro-fluorocopolymer. It is recommended for bonding low dielectric constant PTFE (Teflon® fluorocarbon polymer) microwave stripline packages and other..